20120234211 | METHOD FOR UPGRADING COMBUSTION ASH - A method of producing enhanced coal combustion ash for use in pozzolanic applications or cement manufacture, in which the enhanced combustion ash has lower mercury content. A slurry is formed of the combustion ash and water and is subjected to froth flotation to form a mercury-enriched ash slurry and a mercury-depleted ash slurry. The product mercury-depleted ash slurry is isolated and may optionally be dried. The combustion ash may be pulverized prior to being used to form the slurry, reducing its mean particle size. The mercury-depleted combustion ash product has reduced levels of mercury and ammonia, and reduced particle size. | 09-20-2012 |
20110120348 | UPGRADED COMBUSTION ASH AND ITS METHOD OF PRODUCTION - Described and claimed herein is a method of producing enhanced combustion ash for use in pozzolanic applications or cement clinker manufacture. The method employs a primary process in which wet or dry feedstock is pulverized with sonication using one or more grinding media having a maximum component size of about 2 mm. Alternatively, the media may have a true grinding medium volume to chamber volume ratio of at least 0.29. Also disclosed an claimed is an enhanced combustion ash produced by the method, whereby the enhanced combustion ash has one or more qualities that make it particularly suitable in pozzolanic applications or cement clinker manufacture. | 05-26-2011 |