Patent application number | Description | Published |
20130081589 | METHOD OF MANUFACTURING AN ENGINE BLOCK - A method for manufacturing an engine block includes removing material from the top deck of the engine block surrounding a first opening to create a first recessed area, positioning a first insert within the first recessed area, removing material from the top deck of the engine block surrounding a second opening to create a second recessed area that at least partially overlaps the first recessed area, and positioning a second insert within the second recessed area. | 04-04-2013 |
20130132012 | EDDY CURRENT BASED METHOD FOR COATING THICKNESS MEASUREMENT - A method of configuring an eddy current detector to measure a thickness of a coating on a substrate includes measuring an impedance of the coated substrate, and establishing an impendence plane plot using a computer. The method may also include determining a rotation angle. The rotation angle may be an angle of rotation of the impedance plane plot that will make the inductive reactance component of the impedance substantially insensitive to substrate electrical conductivity within a coating thickness range. The method may further include establishing a calibration curve that is substantially insensitive to substrate electrical conductivity using the rotation angle. The calibration curve may be a curve that relates the inductive reactance component of the impedance to coating thickness. | 05-23-2013 |
20140298987 | Repaired Pistons And Collection Thereof - A repaired piston includes a crown composed of base and welding filler materials, and having an annular rim extending around a combustion bowl. A finite number of repaired defects are within the annular rim, and have a spatial distribution limited by a multidirectional spacing parameter, and a size distribution limited by a unidirectional sizing parameter. | 10-09-2014 |
20140312096 | OXY-FUEL WELD REPAIR OF METALLIC COMPONENTS - A method of repairing a metallic component is disclosed. The method may include machining away a damaged first portion of the component, and machining away a second portion of the component adjacent the damaged first portion, the second portion being an area that would be subject to distortion resulting from solidification of molten weld material added to repair the damaged first portion. The method may also include inserting a dam made of a high-temperature-resistant material adjacent the machined away second portion to contain molten weld material added to the machined away second portion. Oxy-fuel welding may be performed to at least partially fill the machined away damaged first portion of the component and the machined away second portion of the component, and final machining of the welded portions may be performed. | 10-23-2014 |
20140359989 | METHOD OF REMANUFACTURING A SEALING SURFACE - A method of remanufacturing a seal surface includes forming a groove into a component surface at a location of a worn seal surface. A bead of new seal material may then be deposited in the groove by laser cladding. The bead of new seal material may then be machined to form a new seal surface that is generally flush with the component surface. | 12-11-2014 |
20150020932 | METHOD OF REMANUFACTURING A ROCKER ARM - A method of remanufacturing a rocker arm is provided. The rocker arm includes a body defining a center hole for receipt of a shaft, a first arm extending radially away from the center hole, and a second arm extending radially away from the center hole in a direction opposite the first arm. The second arm is configured to be operatively engaged with a valve mechanism and includes a contact surface configured to engage with a braking member. The contact surface includes a worn upper hardened surface. The method includes machining the contact surface to a depth less than a predefined tolerance limit to remove the worn upper hardened surface and create a generally planar unhardened contact surface. The method further includes hardening the unhardened contact surface using a laser to create a repaired contact surface with a surface hardness of greater than at least Rockwell C 50. | 01-22-2015 |
20150069025 | MACHINE COMPONENT CLADDING STRATEGY - Cladding and remanufacturing a machine component includes directing cleaning and welding beams split from an incident laser beam toward the machine component, and moving the machine component relative the cleaning and welding beams such that the welding beam trails behind the cleaning beam along a common travel path. A surface of the machine component is decontaminated by the cleaning beam, whilst a cladding material is melted via the welding beam such that upon solidifying the cladding material forms a coating metallurgically bonded to base material and previously deposited cladding material of the machine component. | 03-12-2015 |
20150122783 | LASER CLADDING WITH A LASER SCANNING HEAD - A method for laser cladding a material onto a surface of a machine component using a laser scanning head with laser scanning optics is disclosed. The method includes forming a molten bead of cladding material by directing a beam with the laser scanning optics over a bead scan on the machine component. The method also includes directing the beam with the laser scanning optics over a secondary scan on the machine component, the secondary scan being offset from the bead scan at a predetermined distance on the machine component. | 05-07-2015 |